Rubber bridge expansion joint Properties | Neoprene ( -25ºC~ 60ºC) | Natural ( -35ºC~ 60ºC) | Neoprene ( -40ºC~ 60ºC) | |
Hardness (IRHD) | 60±5 | 60±5 | 60±5 | |
Tensile Strength (Mpa) | ≥15 | ≥16 | ≥14 | |
Elongation at break (%) | ≥400 | ≥400 | ≥350 | |
Brittleness temperature (ºC) | ≤-40 | ≤-50 | ≤-60 | |
Compression set constant(Room temperature×24h) | ≤20 | ≤20 | ≤20 | |
Resistant Ozone aging (25~ 50pphm) 20% Elongation 40ºC×96h | No cracks | No cracks | No cracks | |
Hot air aging (Compared with previous unaged value occurred biggest change ) | Test conditions (ºC×h) | 70ºC×96h | 70ºC×96h | 70ºC×96h |
Tensile Strength (%) | ±15 | ±15 | ±10 | |
Elongation at break (%) | ±25 | ±25 | ±20 | |
Hardness change(IRHD) | 0~+10 | -5~+10 | 0~+10 | |
Salt water(23ºC×14d, 4%Concentration) | Volume Change (%) | ≤+10 | ≤+10 | ≤+10 |
Hardness Change(IRHD) | ≤+10 | ≤+10 | ≤+10 | |
Rubber and steel bonding peel strength(kN/m) | >7 | >7 | >7 | |
oil resistance(No.1 Standard Oil, 23ºC×168h) | Volume Change (%) | -5~+10 | <+45 | <+45 |
Hardness Change(IRHD) | -10~+5 | <-25 | <-25 |
NO. | Items | Index | |
ElastomerRubberProperty | |||
1 | Hardness (IRHD) | 60±5 | |
2 | Tensile Strength(Mpa) | ≥15 | |
3 | Elongation at break(%) | ≥400 | |
4 | Brittleness temperature(℃) | ≤-40 | |
5 | Compression set constant(Room temperature×24h) | ≤20 | |
6 | Resistant Ozone aging(25~50pphm) | No cracks | |
7 | Hot air aging(Compared with previous unaged value occurred biggest change) | Test conditions(℃×h) | 70℃×96h |
Tensile Strength (%) | ±15 | ||
Eongation at break (%) | ±25 | ||
Hardness change(IRHD) | 0~+10 | ||
8 | Salt water(23℃×14d, %Concentration) | Volume Change(%) | ≤+10 |
Hardness Change (IRHD) | ≤+10 | ||
9 | oil resistance(No.1 Standard Oil,23℃×168h) | Volume Change(%) | -5~+10 |
Hardness Change (IRHD) | -10~+5 | ||
10 | Rubber and steel bonding peel strength(kN/m) | >7 | |
InsideSteelProperty | |||
1 | Steel Yield Strength,N/mm2 | ≥235 | |
2 | Steel Tensile Strength,N/mm2 | 360-510 |